This article focuses on those areas of coatings technology where silicon-based technology (SBT) is the primary enabling technology and where SBT is used as an additive to provide unique properties to the coating film. It describes the chemistry and the uses of alkoxy silanes. The uses of silicates, siliconates, silicone fluids, and silicone resins in coatings are reviewed. The article discusses the various applications of SBT, namely, primers, heat-resistant coatings, industrial maintenance coatings, hygienic coatings, and abrasion-resistant coatings, and for marine biofouling control. It also provides information on the benefits of silicon-base additives.
Gerald L. Witucki, Silicon-Based Technologies in Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 177–184, https://doi.org/10.31399/asm.hb.v05b.a0006028
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.