Skip Nav Destination
ASM Handbook
Protective Organic CoatingsAvailable to Purchase
Edited by
ASM International
Volume
5B
ISBN electronic:
978-1-62708-172-6
Publication date:
2015
Volume 5B addresses the subject of organic protective coatings, the most widely used preventative in the battle with rust and corrosion. It covers the entire spectrum of organic coating materials from acrylics, alkyds, and epoxies to powder coats, waxes, and zinc-rich blends. It compares and contrasts coating properties, describes where and how specific coatings are used, and presents qualification testing and surface preparation procedures. The volume also provides introductory information on chemistry, composition, and the role of pigments, resins, additives, and solvents. For information on the print version of Volume 5B, ISBN: 978-1-62708-081-1, follow this link.
Protective Organic Coatings
Edited by: Kenneth B. Tator
https://doi.org/10.31399/asm.hb.v05b.9781627081726
ISBN (electronic): 978-1-62708-172-6
Publisher: ASM International
Published: 2015
Download citation file:
Table of Contents
-
Introduction
-
Elemental Chemistry IntroductionPublished:30 September 2015
-
Composition of a Paint CoatingPublished:30 September 2015
-
Qualification Testing for Coating System SelectionPublished:30 September 2015
-
Overview of Quality and the Standards, Programs, and Certifications Used in the Coatings IndustryPublished:30 September 2015
-
-
Coating Materials
-
Alkyd ResinsByMichael G. KoehlerMichael G. KoehlerProfessional Analysis and ConsultingSearch for other works by this author on:Published:30 September 2015
-
Acrylic CoatingsByLeo J. ProcopioLeo J. ProcopioThe Dow Chemical CompanySearch for other works by this author on:Published:30 September 2015
-
Epoxy Resins and CurativesPublished:30 September 2015
-
Polyvinylidene Fluoride-Based Coatings TechnologyByRobert A. IezziRobert A. IezziRAI Technical Solutions, Inc.Search for other works by this author on:Published:30 September 2015
-
Fluoroethylene Vinyl Ether Resins for High-Performance CoatingsByKristen BlankenshipKristen BlankenshipAGC Chemicals Americas, Inc.Search for other works by this author on:Published:30 September 2015
-
Polyester and Vinyl Ester CoatingsPublished:30 September 2015
-
Polyurethane CoatingsBySteven Reinstadtler;Steven ReinstadtlerBayer MaterialScience LLCSearch for other works by this author on:C. Todd Williams;C. Todd WilliamsBayer MaterialScience LLCSearch for other works by this author on:Ahren OlsonAhren OlsonBayer MaterialScience LLCSearch for other works by this author on:Published:30 September 2015
-
Polyurea-Based CoatingsByDudley J. Primeaux, IIDudley J. Primeaux, IIVersaFlex Inc.Search for other works by this author on:Published:30 September 2015
-
Polyaspartic CoatingsByEdward P. Squiller;Edward P. SquillerBayer MaterialScience LLCSearch for other works by this author on:Steven ReinstadtlerSteven ReinstadtlerBayer MaterialScience LLCSearch for other works by this author on:Published:30 September 2015
-
Polymeric Floor CoatingsByFrederick GelfantFrederick GelfantThe Stonhard GroupSearch for other works by this author on:Published:30 September 2015
-
Powder Coatings—PipelinesByJ. Alan KehrJ. Alan KehrAlan Kehr Anti-CorrosionSearch for other works by this author on:Published:30 September 2015
-
Powder Coatings—Other IndustriesByDenis GrimshawDenis GrimshawJotun Powder CoatingsSearch for other works by this author on:Published:30 September 2015
-
Silicon-Based Technologies in CoatingsByGerald L. WituckiGerald L. WituckiDow Corning CorporationSearch for other works by this author on:Published:30 September 2015
-
Polysiloxane Hybrid CoatingsByGerald L. WituckiGerald L. WituckiDow Corning CorporationSearch for other works by this author on:Published:30 September 2015
-
Smart Coatings and Nanotechnology Applications in CoatingsByJoshua ArmstrongJoshua ArmstrongTesla Nanocoatings Inc.Search for other works by this author on:Published:30 September 2015
-
Bitumens—Coal Tar and Asphalt CoatingsPublished:30 September 2015
-
Wax-Based Coating SystemsByFrank RamptonFrank RamptonTrenton CorporationSearch for other works by this author on:Published:30 September 2015
-
-
Surface Preparation and Coating Application
-
Surface PreparationPublished:30 September 2015
-
Soluble Salts beneath CoatingsPublished:30 September 2015
-
Shop and Field Quality Control and Quality AssuranceByPublished:30 September 2015
-
Worker Health and Environmental Hazards Associated with Coating Application and RemovalByStanford T. LiangStanford T. LiangAM Health and SafetySearch for other works by this author on:Published:30 September 2015
-
Green CoatingsByBarry LawBarry LawMaster Painters Institute (MPI)Search for other works by this author on:Published:30 September 2015
-
Coating Various SubstratesPublished:30 September 2015
-
-
Industrial Uses
-
Pipeline Industry CoatingsPublished:30 September 2015
-
Marine CoatingsByPublished:30 September 2015
-
Coatings Used in the Nuclear IndustryPublished:30 September 2015
-
Bridge CoatingsPublished:30 September 2015
-
Guidance for the Use of Protective Coatings in Municipal Potable Water SystemsByPublished:30 September 2015
-
Protective Coatings for Corrosion Control in Municipal Wastewater SystemsByPublished:30 September 2015
-
Guidelines for Maintenance Coating of Steel Structures in Pulp and Paper MillsPublished:30 September 2015
-
Coatings for Commercial Structures and Building Deficiencies that Affect PerformanceByKevin D. KnightKevin D. KnightRetro-Specs, Ltd.Search for other works by this author on:Published:30 September 2015
-
-
Coating Analysis and Evaluation
-
Estimating the Cost of Industrial Painting ProjectsPublished:30 September 2015
-
Laboratory TestingByValerie SherbondyValerie SherbondyKTA-Tator, Inc.Search for other works by this author on:Published:30 September 2015
-
Coating Failures and DefectsByPublished:30 September 2015
-
Overview of Other Protection Methods[1]Published:30 September 2015
-