Abstract
This chapter addresses the issue of die failures in hot and cold forging operations. It describes failure classifications, fatigue fracture and wear mechanisms, analytical wear models, and the various factors that limit die life. It also includes several case studies in which finite-element modeling is used to predict die failure and extend die life.
You do not currently have access to this chapter.
Citation
Mark Gariety, Die Failures in Cold and Hot Forging, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 295–317, https://doi.org/10.31399/asm.tb.chffa.t51040295
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Lubrication and Wear in Forging
Friction, Lubrication, and Wear Technology
Friction and Lubrication
Cold and Hot Forging Fundamentals and Applications
Failure in Steel Forging
Failure Analysis of Heat Treated Steel Components
Forging
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear
Hot Upset Forging
Metalworking: Bulk Forming
Process Modeling in Cold Forging Using Finite-Element Analysis
Cold and Hot Forging Fundamentals and Applications
Finite Element Method Applications in Bulk Forming
Metalworking: Bulk Forming
Finite-Element Modeling in Failure Analysis
Failure Analysis and Prevention (2021 Edition)
Cold and Warm Forging
Cold and Hot Forging Fundamentals and Applications
Analysis of Center Burst During Hot Forging
ASM Failure Analysis Case Histories: Processing Errors and Defects