Cold and Hot Forging: Fundamentals and Applications
Edited by
ASM International
ISBN electronic:
978-1-62708-300-3
Publication date:
2005
Abstract
This chapter addresses the issue of die failures in hot and cold forging operations. It describes failure classifications, fatigue fracture and wear mechanisms, analytical wear models, and the various factors that limit die life. It also includes several case studies in which finite-element modeling is used to predict die failure and extend die life.
Topics
Fracture analysis,
Extrusion dies,
Forging dies,
Forging machines,
Metal forming lubricants,
Wrought superalloys,
Billets,
Forgings,
Shearing,
Backward extrusion,
Forward extrusion,
Cold forging,
Die forging,
Hot forging,
Hammer forging,
Press forging,
Radial forging,
Ring forging,
Roll forging,
Rotary forging,
Finite element analysis,
Microstructure modeling,
Forgeability,
Friction and wear properties,
Flow stress,
Plane stress,
Plastic strain,
Engineering strain,
Lubricant analysis,
Fatigue fracture,
Wear
You do not currently have access to this chapter.
Citation
Mark Gariety, Die Failures in Cold and Hot Forging, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 295–317, https://doi.org/10.31399/asm.tb.chffa.t51040295
Download citation file:
Related Book Content
Friction and Lubrication
Cold and Hot Forging Fundamentals and Applications
Lubrication and Wear in Forging
Friction, Lubrication, and Wear Technology
Failure in Steel Forging
Failure Analysis of Heat Treated Steel Components
Hot Upset Forging
Metalworking: Bulk Forming
Process Modeling in Cold Forging Using Finite-Element Analysis
Cold and Hot Forging Fundamentals and Applications
Finite Element Method Applications in Bulk Forming
Metalworking: Bulk Forming
Finite-Element Modeling in Failure Analysis
Failure Analysis and Prevention (2021 Edition)
Cold and Warm Forging
Cold and Hot Forging Fundamentals and Applications
Analysis of Center Burst During Hot Forging
ASM Failure Analysis Case Histories: Processing Errors and Defects
Carbon Steels and Alloy Steels Used in Warm and Hot Working
Induction Heating and Heat Treatment