This chapter discusses the factors that affect die steel selection for hot forging, including material properties such as hardenability, heat and wear resistance, toughness, and resistance to plastic deformation and mechanical fatigue. It then describes the relative merits of various materials and the basic requirements for cold forging dies. The chapter also covers die manufacturing processes, such as high-speed and hard machining, electrodischarge machining, and hobbing, and the use of surface treatments.
Sign in
ASM members
Member Sign InPrashant Mangukia, Die Materials and Die Manufacturing, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 277–293, https://doi.org/10.31399/asm.tb.chffa.t51040277
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.