Skip Nav Destination
ASM Technical Books
Cold and Hot Forging: Fundamentals and Applications
Edited by
ASM International
ISBN electronic:
978-1-62708-300-3
Publication date:
2005
Abstract
Prior to forging, it is often necessary to preform billet stock to achieve adequate material distribution. This chapter discusses the equipment used for such operations, including transverse rolling machines, electric upsetters, ring-rolling mills, horizontal presses, and rotary (orbital) and radial forging machines. It describes their basic operating principles as well as advantages and disadvantages.
Topics
Fracture analysis,
Extrusion dies,
Forging dies,
Forging machines,
Metal forming lubricants,
Wrought superalloys,
Billets,
Forgings,
Shearing,
Backward extrusion,
Forward extrusion,
Cold forging,
Die forging,
Hot forging,
Hammer forging,
Press forging,
Radial forging,
Ring forging,
Roll forging,
Rotary forging,
Finite element analysis,
Microstructure modeling,
Forgeability,
Friction and wear properties,
Flow stress,
Plane stress,
Plastic strain,
Engineering strain,
Lubricant analysis,
Ring rolling mills
You do not currently have access to this chapter.
Citation
Pinak Barve, Special Machines for Forging, Cold and Hot Forging: Fundamentals and Applications, Edited By Taylan Altan, Gracious Ngaile, Gangshu Shen, ASM International, 2005, p 141–150, https://doi.org/10.31399/asm.tb.chffa.t51040141
Download citation file: