Beryllium Chemistry and Processing
Chapter 17: Mechanical Properties of Beryllium
-
Published:2009
Abstract
This chapter describes the effect of processing variables on the mechanical properties of beryllium, including tensile and yield strength, fracture toughness, creep and fatigue strength, ductile-to-brittle transition, and notch sensitivity. It also discusses the effects of chemical composition, impurities, and grain size and the use of hydrostatic testing.
Alfred Goldberg, David L. Olson, Mechanical Properties of Beryllium, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 209–252, https://doi.org/10.31399/asm.tb.bcp.t52230209