Chapter 3: Sources of Beryllium
Retired
-
Published:2009
Abstract
Beryllium is the 44th most abundant element on Earth, with an estimated concentration of six parts per million in the Earth’s crust. It is found in various forms in more than 100 minerals, two of which, beryl and bertrandite, account for most of the beryllium produced throughout the world. This chapter describes where and how beryllium is obtained and provides facts, figures, and insights on global supply and demand.
Sign in
ASM members
Member Sign InKenneth A. Walsh, Edgar E. Vidal, Sources of Beryllium, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 19–26, https://doi.org/10.31399/asm.tb.bcp.t52230019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.