This chapter describes some of events and developments that helped drive the commercialization of beryllium and its acceptance as an engineering material. It traces the growth of the domestic beryllium industry from its origins in the 1920s to the present time, and provides a status update on the primary beryllium producers throughout the world.
Sign in
ASM members
Member Sign InKenneth A. Walsh, Donald J. Kaczynski, Loren A. Jacobson, David L. Olson, History of Beryllium, Beryllium Chemistry and Processing, By Kenneth A. Walsh;Edited By Edgar E. Vidal, Alfred Goldberg, Edward N.C. Dalder, David L. Olson, Brajendra Mishra, ASM International, 2009, p 7–18, https://doi.org/10.31399/asm.tb.bcp.t52230007
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.