Introduction to Coating Design and Processing Available to Purchase
-
Published:2013
Abstract
This article begins with a description of the advantages and disadvantages of thermal spraying. It provides a discussion on the importance of substrate processing prior to coating and the role of undercutting in repair. The article reviews the steps for substrate preparation, namely, cleaning, roughening, masking, and preheating. Information on the equipment and process variables of dry abrasive grit blasting are also provided. The article describes the roles of spray stream and the spray pattern for all thermal spray processes. It discusses the defects arising from poor temperature control and from the variables influencing the manipulation of the spray torch. The article concludes with helpful information on calculating the process efficiency of thermal spraying.
Introduction to Coating Design and Processing, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 76–88, https://doi.org/10.31399/asm.hb.v05a.a0005725
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.