Biomedical Coatings Made by Thermal Spraying for Orthopaedic Joint Applications
-
Published:2013
Abstract
This article provides an overview of how thermal spray technology has adapted to meet the needs of the orthopaedic industry. It includes the challenges facing the development of artificial joints, substrate material selection criteria, thermal spray solutions, and clinical outcomes of thermal spray coatings. The article focuses on plasma thermal spray, which is the technique most often used to make porous titanium and hydroxyapatite (HA) coatings, such as thermal spray titanium, thermal spray HA, solution-precipitated HA, thermal spray chromium oxide, and thermal spray chromium carbide cermet coatings.
Sign in
ASM members
Member Sign InZongtao Zhang, Biomedical Coatings Made by Thermal Spraying for Orthopaedic Joint Applications, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 306–311, https://doi.org/10.31399/asm.hb.v05a.a0005741
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!