Replacement for Hard Chrome Plating on Aircraft Landing Gear[1] Available to Purchase
-
Published:2013
Abstract
High-velocity oxyfuel (HVOF)-applied thermal spray coatings are viable candidates for replacement of hard chrome in numerous applications. HVOF thermal spraying can be used to deposit both metal alloy and cermet coatings that are dense and highly adherent to all the commonly used base metals in airframe structures. This article summarizes the results of materials and component testing. It also presents a cost/benefit analysis of HVOF WC/17Co and WC/10Co4Cr coatings on aircraft landing gear components.
Mark Pollack, Replacement for Hard Chrome Plating on Aircraft Landing Gear, Thermal Spray Technology, Vol 5A, ASM Handbook, Edited By Robert C. Tucker, Jr., ASM International, 2013, p 296–297, https://doi.org/10.31399/asm.hb.v05a.a0005739
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.