Thermal Spray TechnologyAvailable to Purchase
Volume 5A provides an introduction to thermal spray technology including plasma spray, high velocity oxy-fuel, and detonation gun deposition. It explains how each process works and the types of coating materials typically used. It also addresses critical application issues, including substrate requirements, surface preparation, bonding agents, adhesion, and uniformity, and their effect on surface properties, wear, corrosion, and thermal barrier performance. The volume also provides practical information on how to test and analyze thermal spray coatings and it presents several examples of how thermal spray technology is being used. For information on the print version of Volume 5A, ISBN: 978-1-61503-996-8, follow this link.
Download citation file:
Table of Contents
-
Introduction to Thermal Spray Technology and Surface Engineering
-
Introduction to Thermal Spray TechnologyByR.C. Tucker, Jr.R.C. Tucker, Jr.The Tucker Group
Revising author
Search for other works by this author on:Published:01 August 2013 -
Surface Engineering[1]ByR.C. Tucker, Jr.R.C. Tucker, Jr.The Tucker GroupSearch for other works by this author on:Published:01 August 2013
-
-
Thermal Spray Processes and Coatings
-
Thermal Spray ProcessesByDaryl E. CrawmerDaryl E. CrawmerThermal Spray Technologies, Inc.Search for other works by this author on:Published:01 August 2013
-
Cold Spray ProcessByJeganathan KarthikeyanJeganathan Karthikeyan
Revising author
Search for other works by this author on:Published:01 August 2013 -
Coating Structures, Properties, and MaterialsByDaryl E. CrawmerDaryl E. CrawmerThermal Spray Technologies Inc.Search for other works by this author on:Published:01 August 2013
-
Process Control and Control EquipmentByDaryl E. CrawmerDaryl E. CrawmerThermal Spray Technologies Inc.
Revising author
Search for other works by this author on:Published:01 August 2013
-
-
Consumables
-
Feedstock Material Considerations for Thermal SprayByNoppakun Sanpo;Noppakun SanpoSwinburne University of TechnologySearch for other works by this author on:Christopher C. BerndtChristopher C. BerndtSwinburne University of Technology and Stony Brook UniversitySearch for other works by this author on:Published:01 August 2013
-
-
Precoating and Postcoating Processing
-
Precoating Operations[1]Published:01 August 2013
-
Postcoating OperationsPublished:01 August 2013
-
-
Health and Safety
-
Health and SafetyByDaryl E. CrawmerDaryl E. CrawmerThermal Spray Technologies, Inc.
Revising author
Search for other works by this author on:Published:01 August 2013
-
-
Testing and Characterization
-
Introduction to Testing and CharacterizationByDana RuckerDana RuckerSiemens
Revising author
Search for other works by this author on:Published:01 August 2013 -
Metallography and Image AnalysisPublished:01 August 2013
-
Testing of CoatingsByKen CouchKen CouchProtech Lab CorporationSearch for other works by this author on:Published:01 August 2013
-
Powder Testing and CharacterizationByPublished:01 August 2013
-
-
Existing and New Market Opportunities in Thermal Spray Applications
-
Introduction to Applications for Thermal Spray ProcessingByMitchell R. DorfmanMitchell R. DorfmanSulzer Metco (U.S.) Inc.Search for other works by this author on:Published:01 August 2013
-
Corrosion Control for Marine- and Land-Based Infrastructure ApplicationsByShiladitya PaulShiladitya PaulTWI, Cambridge, United KingdomSearch for other works by this author on:Published:01 August 2013
-
Corrosion and Wear Control for Industrial Applications[1]ByMitchell R. DorfmanMitchell R. DorfmanSulzer Metco (U.S.) Inc.
Revising author
Search for other works by this author on:Published:01 August 2013 -
Thermal Spray Coatings for Electrical and Electronic ApplicationsByAtin SharmaAtin SharmaSulzer Metco (U.S.) Inc.Search for other works by this author on:Published:01 August 2013
-
Thermal and Environmental Barrier Coatings (TBCs/EBCs) for Turbine EnginesByRogerio S. Lima;Rogerio S. LimaNational Research Council of Canada (NRC)Search for other works by this author on:Dongming Zhu;Dongming ZhuNational Aeronautics and Space Administration (NASA)Search for other works by this author on:Li LiLi LiPraxair Surface TechnologiesSearch for other works by this author on:Published:01 August 2013
-
Thermal Spray Technology Growth in Gas Turbine ApplicationsByMitchell R. Dorfman;Mitchell R. DorfmanSulzer Metco (U.S.) Inc.Search for other works by this author on:P. MeyerP. MeyerSulzer Metco (U.S.) Inc.Search for other works by this author on:Published:01 August 2013
-
Abradable Thermal Spray Applications and TechnologyByScott WilsonScott WilsonSulzer Metco (Switzerland)Search for other works by this author on:Published:01 August 2013
-
Replacement for Hard Chrome Plating on Aircraft Landing Gear[1]ByPublished:01 August 2013
-
Automotive Coatings and ApplicationsByNoritaka MiyamotoNoritaka MiyamotoToyota Motor CorporationSearch for other works by this author on:Published:01 August 2013
-
Biomedical Coatings Made by Thermal Spraying for Orthopaedic Joint ApplicationsByZongtao ZhangZongtao ZhangStryker Howmedica OsteonicsSearch for other works by this author on:Published:01 August 2013
-
Protective Overlays and Coatings Used in Oil SandsByGary Fisher;Gary FisherAlberta Innovates—Technology FuturesSearch for other works by this author on:Tonya WolfeTonya WolfeAlberta Innovates—Technology FuturesSearch for other works by this author on:Published:01 August 2013
-
Renewable Energy ApplicationsByRobert Vassen;Robert VassenForschungszentrum Jülich Institute of Energy and Climate Research (IEK-1)Search for other works by this author on:Georg MauerGeorg MauerForschungszentrum Jülich Institute of Energy and Climate Research (IEK-1)Search for other works by this author on:Published:01 August 2013
-
Nuclear Industry Applications for Thermal SprayByKendall J. HollisKendall J. HollisLos Alamos National LaboratorySearch for other works by this author on:Published:01 August 2013
-
Thermal Spray Applications in the Steel IndustryByCharles M. KayCharles M. KayASB Industries, Inc.Search for other works by this author on:Published:01 August 2013
-
Thermal Spray Applications in the Paper Production Industry[1]ByMitchell R. Dorfman;Mitchell R. DorfmanSulzer Metco (U.S.) Inc.
Revising author
Search for other works by this author on:Atin SharmaAtin SharmaSulzer Metco (U.S.) Inc.Revising author
Search for other works by this author on:Published:01 August 2013 -
Printing Industry Applications[1]ByAtin SharmaAtin SharmaSulzer Metco (U.S.) Inc.
Revising author
Search for other works by this author on:Published:01 August 2013 -
Additional Applications in Thermal SprayByMitchell R. DorfmanMitchell R. DorfmanSulzer Metco (U.S.) Inc.
Revising author
Search for other works by this author on:Published:01 August 2013
-
-
Reference Information
-
Guide to General Information SourcesByR.C. Tucker, Jr.R.C. Tucker, Jr.The Tucker Group
Revising author
Search for other works by this author on:Published:01 August 2013 -
A Brief History of the Development of Thermal Spray Processes and MaterialsByR.C. Tucker, Jr.R.C. Tucker, Jr.The Tucker Group
Revising author
Search for other works by this author on:Published:01 August 2013
-