Additive Manufacturing of Cobalt Alloys Available to Purchase
-
Published:2020
Abstract
Traditional processing methods for the part production of Co-Cr alloys include casting, powder metallurgy, and metal forming. However, the steps involved during materials processing followed by metal forming and machining are time consuming and fraught with processing variables. Three-dimensional (3D) printing enables rapid evolution in design, personalization, and so on. This article presents a brief description of some common additive manufacturing (AM) processes for the production of cobalt alloy parts, and provides a comparison between AM and conventional processing methods. The discussion is centered on process-microstructure-properties correlation in additively manufactured cobalt alloys and applications of these alloys.
Amir Mostafaei, Jerard V. Gordon, Anthony D. Rollett, Additive Manufacturing of Cobalt Alloys, Additive Manufacturing Processes, Vol 24, ASM Handbook, Edited By David L. Bourell, William Frazier, Howard Kuhn, Mohsen Seifi, ASM International, 2020, p 374–379, https://doi.org/10.31399/asm.hb.v24.a0006573
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.