Binder Jetting and Sintering in Additive Manufacturing Available to Purchase
-
Published:2020
Abstract
This article focuses on binder-jetting technologies in additive manufacturing (AM) that produce metal artifacts either directly or indirectly. The intent is to focus on the most strategic and widespread uses of the binder jetting technology and review some of the challenges and opportunities for that technology. The discussion includes a historical overview and covers the major steps involved and the advantages of using the binder jetting process. The major steps of the process covered include printing, curing, de-powdering, and sintering.
Amy Elliott, Corson Cramer, Binder Jetting and Sintering in Additive Manufacturing, Additive Manufacturing Processes, Vol 24, ASM Handbook, Edited By David L. Bourell, William Frazier, Howard Kuhn, Mohsen Seifi, ASM International, 2020, p 239–246, https://doi.org/10.31399/asm.hb.v24.a0006569
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.