Abstract
This appendix is a collection of selected continuous cooling transformation diagrams for carbon steels; Mn steels; Mn-Mo, Mn-Ce, Mn-Ni-Mo, and Mn-Ni-CrMo steels; silicon steels; nickel steels; Ni-Cr-Mo steels; and chromium steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Continuous Cooling Diagrams of Selected Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 601–627, https://doi.org/10.31399/asm.tb.fahtsc.t51130601
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
The History of Engineering Alloy Steels
The History of Metals in America
Isothermal Diagrams of Selected Steels
Failure Analysis of Heat Treated Steel Components
Heat Treatment
Metals Fabrication Understanding the Basics
Magnetically Soft Materials
Metals Handbook Desk Edition (2nd Edition)
Internal Cracks in Cast Steel With 9% Ni for Cryogenic Applications
Handbook of Case Histories in Failure Analysis
Physical Properties of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Classification and Designation of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hardenability of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Physical Properties of Carbon and Low-Alloy Steels
Failure Analysis of Heat Treated Steel Components
Failure of Four Cast Steel Gear Segments
Handbook of Case Histories in Failure Analysis