Skip Nav Destination
View Technical Books >
ASM Technical Books
Failure Analysis of Heat Treated Steel Components
ASM International
ISBN electronic:
978-1-62708-284-6
Publication date:
2008
Book Chapter
Appendix 10: Isothermal Diagrams of Selected Steels
-
Published:2008
Abstract
This appendix is a collection of isothermal diagrams for carbon steels, chromium-molybdenum steels, nickel-chromium-molybdenum steels, nickel-molybdenum steels, and chromium steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Isothermal Diagrams of Selected Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 587–599, https://doi.org/10.31399/asm.tb.fahtsc.t51130587
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Continuous Cooling Diagrams of Selected Steels
Failure Analysis of Heat Treated Steel Components
Elevated-Temperature Properties of Ferritic Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Severe General Corrosion on Historic Lane Plate Made From Chromium Steel
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Failure of Recuperator with Austenitically Welded Pipes
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Failure Analysis of Open End Wrenches Containing Forging Defects
Handbook of Case Histories in Failure Analysis
Brittle Cracking of a Cylindrical Spiral Gear of Axle Gearbox
Handbook of Case Histories in Failure Analysis
Physical Properties of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Fracture and Wear Failure of a Locomotive Turbocharger-Bearing Sleeve
Handbook of Case Histories in Failure Analysis
Classification and Designation of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Physical Properties of Carbon and Low-Alloy Steels
Failure Analysis of Heat Treated Steel Components