Appendix 10: Isothermal Diagrams of Selected Steels
-
Published:2008
Abstract
This appendix is a collection of isothermal diagrams for carbon steels, chromium-molybdenum steels, nickel-chromium-molybdenum steels, nickel-molybdenum steels, and chromium steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Isothermal Diagrams of Selected Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 587–599, https://doi.org/10.31399/asm.tb.fahtsc.t51130587
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Continuous Cooling Diagrams of Selected Steels
Failure Analysis of Heat Treated Steel Components
Elevated-Temperature Properties of Ferritic Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Severe General Corrosion on Historic Lane Plate Made From Chromium Steel
ASM Failure Analysis Case Histories: Medical and Biomedical Devices
Failure of Recuperator with Austenitically Welded Pipes
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Failure Analysis of Open End Wrenches Containing Forging Defects
Handbook of Case Histories in Failure Analysis
Physical Properties of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Brittle Cracking of a Cylindrical Spiral Gear of Axle Gearbox
Handbook of Case Histories in Failure Analysis
Classification and Designation of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hardenability of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Physical Properties of Carbon and Low-Alloy Steels
Failure Analysis of Heat Treated Steel Components