Appendix 7: AISI to Non-AISI Steel Cross Reference
-
Published:2008
Abstract
This appendix contains a table listing cross-references of standard SAE carbon and low-alloy steels to selected chemically similar steels.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
AISI to Non-AISI Steel Cross Reference, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 551–562, https://doi.org/10.31399/asm.tb.fahtsc.t51130551
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Non-AISI to AISI Steel Cross Reference
Failure Analysis of Heat Treated Steel Components
Stress-Corrosion Cracking of Carbon and Low-Alloy Steels (Yield Strengths Less Than 1241 MPa)
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Austenitizing Temperatures for Steels
Failure Analysis of Heat Treated Steel Components
Classification of Carbon and Low-Alloy Steels
Practical Heat Treating Basic Principles
Hardenability Calculation of Carbon and Low-Alloy Steels with Low or Medium Carbon
Steel Heat Treating Fundamentals and Processes
Corrosion of Carbon Steel and Low-Alloy Steel Weldments
Corrosion of Weldments
Failures Related to Welding
Analysis and Prevention of Component and Equipment Failures
Dissimilar Welds With Stainless Steels
Welding, Brazing, and Soldering
Stress Rupture Failures
Failure Investigation of Boiler Tubes A Comprehensive Approach
Steel Products and Properties
Metallurgy for the Non-Metallurgist (Second Edition)