Appendix 6: Physical Properties of Carbon and Low-Alloy Steels
-
Published:2008
Abstract
This appendix is a collection of tables listing coefficients of linear thermal expansion for carbon and low-alloy steels, presenting a summary of thermal expansion, thermal conductivity, and heat capacity; and listing thermal conductivities and specific heats of carbon and low-alloy steels.
You do not currently have access to this chapter.
Citation
Physical Properties of Carbon and Low-Alloy Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 541–550, https://doi.org/10.31399/asm.tb.fahtsc.t51130541
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Physical Properties of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Classification and Designation of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Flux Cored Arc Welding
Welding Fundamentals and Processes
Procedure Development and Practice Considerations for Ultrasonic Welding
Welding, Brazing, and Soldering
Elevated-Temperature Properties of Ferritic Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Service Characteristics of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Fatigue Resistance of Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hardenability of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Physical and Nuclear Properties
Beryllium Chemistry and Processing
Procedure Development and Practice Considerations for Diffusion Welding
Welding, Brazing, and Soldering