This appendix is a collection of tables listing examples of published hardness conversion equations, approximate Rockwell B and C hardness conversion numbers for nonaustenitic steels, and equivalent hardness numbers for Brinell hardness numbers and Vickers (diamond pyramid) hardness numbers for steel.