This chapter briefly outlines some of the basic aspects of failure analysis, describing some of the basic steps and major concerns in conducting a failure analysis. A brief review of failure types from fracture, distortion, wear-assisted failure, and environmentally assisted failure (corrosion) is also provided.
Waldek Wladimir Bose-Filho, José Ricardo Tarpani, Marcelo Tadeu Milan, General Aspects of Failure Analysis, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 111–132, https://doi.org/10.31399/asm.tb.fahtsc.t51130111