High Pressure Cold Spray: Principles and Applications
Chapter 11: Cold Spray Applications in Repair and Refurbishment for the Aerospace, Oil and Gas, and Power-Generation Industries
-
Published:2016
Abstract
This chapter focuses on high-pressure cold spray applications pertaining to repair and refurbishment in the aerospace, oil and gas, and power-generation industries, the last specifically involving repair of gas turbine components. Advantages of cold spray coating in the repair and refurbishment of structural engineering components are also discussed.
D. Srinivasan, Cold Spray Applications in Repair and Refurbishment for the Aerospace, Oil and Gas, and Power-Generation Industries, High Pressure Cold Spray: Principles and Applications, Edited By Charles M. Kay, J. Karthikeyan, ASM International, 2016, p 277–305, https://doi.org/10.31399/asm.tb.hpcspa.t54460277
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.