Modeling and Simulation of Stresses and Distortion in Induction Hardened Steels Available to Purchase
-
Published:2014
Abstract
This article provides a discussion on the analytical modeling and simulation of residual stress states developed in steel parts and the reasons for these varied final stress states. It illustrates how the metallurgical phase transformation of steel alloys can be applied in the simulation of induction hardening processes and the role of these phase transformations in affecting stress and distortion. Emphasis is placed on induction surface hardening, which is the main application of induction heating in steel heat treatment. The article concludes with examples of induction surface-hardened shafts and through-hardened shafts made of plain carbon steel, alloy steel, and limited hardenability steel.
B. Lynn Ferguson, Zhichao Li, Modeling and Simulation of Stresses and Distortion in Induction Hardened Steels, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 272–290, https://doi.org/10.31399/asm.hb.v04c.a0005882
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.