Abstract
This article provides a detailed discussion on the components of a high-performance induction crucible furnace system, namely, furnace body, power supply, and peripheral components. The furnace body contains refractory lining, coil and transformer yokes, and tilting frame and furnace cover. The power supply consists of the following: transformers, frequency converters, capacitor banks, and power cables and furnace coils. The peripheral components comprise recooling device, charging system, and skimming devices. The article also presents a three-dimensional representation of the induction crucible furnace system.
Erwin Dötsch, Bernard Nacke, Components and Design of Induction Crucible Furnaces, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 447–461, https://doi.org/10.31399/asm.hb.v04c.a0005899
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.