Induction heating has the ability to concentrate the electromagnetic field and heat within a certain area of the workpiece. This article provides a detailed discussion on the end heating of bars, rods, and billets using solenoid inductors, oval inductors, and channel inductors. It reviews the importance of computer modeling in predicting the impact of different, interrelated, and nonlinear factors on the transitional and final thermal conditions of billets and bars. The article describes the most appropriate processes to improve end heating process effectiveness. Induction bending of narrow circumferential band of pipe or tube is also discussed. The article concludes...
Sign in
ASM members
Member Sign InValery Rudnev, Induction Heating of Selective Regions, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 346–358, https://doi.org/10.31399/asm.hb.v04c.a0005891
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!