Operation of Induction Furnaces for Steel and Non-iron Materials
-
Published:2014
Abstract
Crucible furnaces, as compared to electric arc furnaces, are increasingly deployed in various melting practices due to their environmental and workplace friendliness and their process benefits. This article focuses on the application of induction crucible furnaces for melting and pouring operations in small-and medium-sized steel foundries, including aluminum, copper, and zinc industries. It also provides information on the process engineering benefits of melting and pouring operations.
Erwin Dötsch, Operation of Induction Furnaces for Steel and Non-iron Materials, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 521–534, https://doi.org/10.31399/asm.hb.v04c.a0005905