Abstract
This article focuses on the aging characteristics of solution and precipitation heat treated aluminum alloy systems and their corresponding types. It includes information on aluminum-copper systems, aluminum-copper-magnesium systems, aluminum-magnesium-silicon systems, aluminum-zinc-magnesium systems, aluminum-zinc-magnesium-copper systems, and aluminum-lithium alloys.
You do not currently have access to this chapter.
Citation
Heat Treatment Practices of Age-Hardenable Aluminum Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 245–273, https://doi.org/10.31399/asm.hb.v04e.a0006288
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
Heat Treatment of Aluminum Alloy Castings
Heat Treating of Nonferrous Alloys
Metallurgy of Heat Treatable Aluminum Alloys
Aluminum Science and Technology
Heat Treatment Metallurgy of Nickel-Base Alloys
Heat Treating of Nonferrous Alloys
Hardness and Electrical Conductivity Testing of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Heat Treating of Titanium and Titanium Alloys
Heat Treating of Nonferrous Alloys
Quenching of Aluminum Alloys
Aluminum Science and Technology
Aluminum Alloy Nomenclature and Temper Designations
Heat Treating of Nonferrous Alloys
Age Hardening of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Annealing of Aluminum and Its Alloys
Heat Treating of Nonferrous Alloys
Heat Treatment of Aluminum Castings
Aluminum Alloy Castings Properties, Processes, and Applications