This article provides a detailed discussion on heat treatment of titanium alloys such as alpha alloys, alpha-beta alloys, and beta and near-beta alloys. Common processes include stress-relief, annealing, solution treating, aging, quenching, and age hardening. It provides information on the effects of alloying elements on alpha/beta transformation. The article also discusses the heat treating procedures, and the furnaces used for heat treating titanium and titanium alloys.
Charles Carson, Heat Treating of Titanium and Titanium Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 511–534, https://doi.org/10.31399/asm.hb.v04e.a0006283