Principles of Heat Treating of Nonferrous Alloys[1]
-
Published:2016
Abstract
This article introduces the mechanism of diffusion and the common types of heat treatments such as annealing and precipitation hardening, which are applicable to most ferrous and nonferrous systems. Three distinct processes occur during annealing: recovery, recrystallization, and grain growth. The article also describes the various types of solid-state transformations such as isothermal transformation and athermal transformation, resulting from the heat treatment of nonferrous alloys. It provides information on the homogenization of chemical composition within a cast structure.
Sign in
ASM members
Member Sign InPrinciples of Heat Treating of Nonferrous Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 3–31, https://doi.org/10.31399/asm.hb.v04e.a0006250
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.