Abstract
Bronzes generally are used to describe many different copper-base alloys in which the major alloying addition is neither zinc nor nickel. They are generally classified by their major alloying elements, for example, tin bronzes with phosphorus used as a deoxidizer, aluminum bronzes, nickel-aluminum bronzes, silicon bronzes, and beryllium bronzes. This article briefly discusses the types, hardening mechanisms, heat treatment processes, applications, and mechanical properties of these bronzes and high-copper alloys.
You do not currently have access to this chapter.
Citation
Sabit Ali, Heat Treating of Bronzes, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 355–396, https://doi.org/10.31399/asm.hb.v04e.a0006281
Download citation file:
Related Book Content
Beryllium-Copper and Other Beryllium-Containing Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Heat Treatment of Nonferrous Alloys
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treatment of Cast Nickel-Base Alloys
Heat Treating of Nonferrous Alloys
Cyclic Stress-Strain Response and Microstructure
Fatigue and Fracture
Heat Treatment of Aluminum and Other Nonferrous Alloys
Practical Heat Treating Basic Principles
Failure of Silicon Bronze Impeller from Dealloying Via Desiliconification
Handbook of Case Histories in Failure Analysis
Heat Treatable Nonferrous Alloys
Heat Treating of Nonferrous Alloys
Metallurgy of Heat Treatable Aluminum Alloys
Heat Treating of Nonferrous Alloys
Annealing and Recrystallization of Coppers
Heat Treating of Nonferrous Alloys
Non-Martensitic Strengthening of Medium-Carbon Steels—Microalloying and Bainitic Strengthening
Steels: Processing, Structure, and Performance (Second Edition)