Brasses are copper alloys with zinc as the principal alloying element. This article provides information on the chemical compositions and mechanical properties of the three types of brasses: alpha, duplex and beta. It briefly discusses the Unified Numbering System designations, compositions, and classifications of wrought brasses and cast brasses. The article provides a discussion on annealing, recrystallization, and grain growth of wrought brasses. Stress relief of wrought brasses, which is typically conducted below the annealing temperatures, is also briefly described.