Heat Treating of Magnesium Alloys[1] Available to Purchase
Revising author
-
Published:2016
Abstract
Magnesium alloys are used predominantly for high-pressure die-cast applications in which the use of a deliberate heat treatment is uncommon. This article provides information on the heat treatment designations for magnesium alloys. It describes the effects of grain size on magnesium alloys and the relationship between hardness and mechanical properties of the alloys. The article discusses the effects of elements such as aluminum, zinc, manganese, rare earths, and yttrium, on precipitation hardening. It describes the types of heat treatment for magnesium alloys, including annealing, stress relieving, solution treating and aging, and reheat treating. The article also discusses the preventive measures for the common problems encountered in heat treating magnesium alloys; and the evaluation of the effectiveness of heat treating procedures. In addition, it presents the processing steps involved in the heat treatment of magnesium alloys and in the prevention and control of magnesium fires.
Trevor Abbott, Heat Treating of Magnesium Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 640–649, https://doi.org/10.31399/asm.hb.v04e.a0006254
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.