Heat Treating of Nonferrous Alloys
Modeling and Simulation of the Heat Treatment of Aluminum Alloys
-
Published:2016
Abstract
Heat treatment simulation helps to predict heat treatment results such as component microstructures, properties, residual stresses, and distortion, and thereby assists in reducing experimental effort in defining heat treatment parameters. This article discusses the modeling and simulation of age hardening as being the most important heat treatment to strengthen aluminum alloys. It provides information on the heat treatment simulation model, the yield strength model based on the responsible strengthening mechanisms, and the flow curve model based on mechanical tests. The article also discusses simulation of the quenching process, and provides examples for aluminum quenching simulation.
Sign in
ASM members
Member Sign InMichael Reich, Olaf Kessler, Modeling and Simulation of the Heat Treatment of Aluminum Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 296–301, https://doi.org/10.31399/asm.hb.v04e.a0006271
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.