Heat Treating of Nonferrous Alloys
Heat Treating of Titanium and Its Alloys
-
Published:2016
Abstract
This article introduces the different types, distinctions, and grades of commercially pure titanium and titanium alloys. It describes three types of alloying elements: alpha stabilizers, beta stabilizers, and neutral additions. The article discusses the basic categories of titanium alloys, namely, alpha and near-alpha titanium alloys, beta and near-beta titanium alloys, and alpha-beta titanium alloys. It also describes the general microstructural features of titanium alloys.
Abstract
This article provides a detailed discussion on the heat treatment processes for titanium and titanium alloys. These processes are age hardening, solution treatment, aging, and annealing. The article illustrates the characteristics of equilibrium phase...
Sign in
ASM members
Member Sign InHeat Treating of Titanium and Its Alloys, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.