A successful heat treating operation is determined by the ability to satisfy the customer's quality requirements consistently and economically. This chapter reviews the steps that are important to produce quality parts in heat treating with a brief practical explanation of each. The steps include selecting proper material and design of the part being treated; determining whether the process is capable of heat treatment; using statistical process control, control charting, and in-process inspection and testing; and applying statistical quality control and final testing (sampling) to verify the results.