Metals are used in many engineering applications because of their mechanical properties, particularly strength and ductility. This chapter explains how mechanical properties are measured and how to interpret the results. It describes the most widely used tests, including tensile tests; Rockwell, Brinell, Vickers, and Knoop hardness tests; and Charpy V-notch impact tests. The chapter also provides information on loading conditions that can lead to fatigue failure, and in some cases, counteract or prevent it.