This chapter examines boiler tube failures attributed to operation-related causes. It discusses failures due to rapid start-ups, excessive load swing, excessive heat inputs, poor water chemistry control, and water-treatment methods.

You do not currently have access to this chapter.
Don't already have an account? Register

2018. "Operation-Related Failures", Failure Investigation of Boiler Tubes: A Comprehensive Approach, Paresh Haribhakti, P.B. Joshi, Rajendra Kumar