Abstract

This chapter provides an outline of the failure modes and mechanisms associated with most boiler tube failures in coal-fired power plants. Primary categories include stress rupture failures, water-side corrosion, fire-side corrosion, fire-side erosion, fatigue, operation failures, and insufficient quality control.