Abstract

This appendix is a table of metric conversions for properties and measurements that commonly apply to metals and alloys.

Abstract

This appendix explains how to calculate atomic packing factors, lattice parameters, and coordination numbers for cubic crystal structures, including simple, body-centered, and face-centered cubic systems. It also addresses hexagonal close-packed systems.

Abstract

This appendix explains how to identify crystallographic planes and directions. It shows how Miller indices, a system for specifying crystallographic planes within a unit cell, are determined for cubic and hexagonal systems. It also explains how x-ray diffraction techniques are used in the study of crystalline structures.

You do not currently have access to this chapter.
Don't already have an account? Register

2008. "Reference Information", Elements of Metallurgy and Engineering Alloys, F.C. Campbell

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal