Elements of Metallurgy and Engineering Alloys
Chapter 10: The Iron-Carbon System
-
Published:2008
Abstract
This chapter examines the isothermal phase transformations of the iron-carbide system. The discussion includes the formation of ferritic, eutectoid, hypoeutectoid, hypereutectoid, bainitic, and martensitic microstructures as well as their properties, composition, and metallurgy. The use of time-temperature-transformation (TTT) diagrams in understanding the phase transformations and the changes in the isothermal transformation curves due to the addition of carbon and other alloying elements are also discussed.
Sign in
ASM members
Member Sign In2008. "The Iron-Carbon System", Elements of Metallurgy and Engineering Alloys, F.C. Campbell
Download citation file: