7255: High-Strength, Fatigue-Resistant Plate
-
Published:2019
Abstract
This datasheet provides information on composition limits for aluminum alloy 7255, with emphasis on the minimum static properties of aluminum alloy 7255 plate and fracture toughness of aluminum alloy 7255-T7751. Fatigue crack growth resistance of alloy 7255 plate is compared with those of legacy alloy 7055 plate.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
7255: High-Strength, Fatigue-Resistant Plate, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 453, https://doi.org/10.31399/asm.hb.v02b.a0006744
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.