Abstract

The aluminum alloy 7099 is a Kaiser aluminum high-strength Al-Mg-Zn-Cu alloy with zirconium that offers a less quench-sensitive alloy for properties in thicker sections for airframe structures such as wing ribs, spars, and skins, as well as fuselage frames and floor beams. This datasheet provides information on key alloy metallurgy and processing effects on mechanical properties of this 7xxx series alloy.

You do not currently have access to this chapter.
Don't already have an account? Register

7099: High-Strength Plate, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 444–445, https://doi.org/10.31399/asm.hb.v02b.a0006741