2195: Al-Li Plate Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy and processing effects on mechanical properties of Al-Li plate alloy 2195. A figure provides a performance comparison of 2195-T84 and 2219-T87 alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
2195: Al-Li Plate Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 316, https://doi.org/10.31399/asm.hb.v02b.a0006608
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.