Skip to Main Content
Skip Nav Destination

Abstract

This article illustrates the relationships among commonly used 2xxx series alloys. It contains tables that list values for composition limits of aluminum-lithium alloys, and aerospace alloys and their temper conditions according to primary design requirements.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal