333.0 and A333.0: Al-Si-Cu Permanent-Mold Casting Alloy
-
Published:2019
Abstract
Alloys 333.0 and A333.0 are age-hardenable permanent mold casting alloys recommended for high-temperature applications requiring pressure tightness. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, fabrication characteristics, and application characteristics of these 3xxx series alloys.
Sign in
ASM members
Member Sign In333.0 and A333.0: Al-Si-Cu Permanent-Mold Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 538–539, https://doi.org/10.31399/asm.hb.v02b.a0006564