Skip to Main Content
Skip Nav Destination

Abstract

The aluminum alloys 319.0, A319.0, B319.0, and 320.0 offer good strength in the as-cast condition. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, fabrication characteristics, and applications of these 3xxx series alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

319.0, A319.0, B319.0, and 320.0: Al-Si-Cu General Purpose Foundry Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 533–535, https://doi.org/10.31399/asm.hb.v02b.a0006562

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal