Abstract

This datasheet provides information on composition limits, processing effects on physical and mechanical properties, and fabrication characteristics of electrical bus conductor aluminum alloys 6101 and 6201 along with standard temper designations. Machining and forming characteristics of alloy 6101 are compared with related alloys and tempers.