Abstract

The aluminum alloys 383.0, 384.0, and A384.0 are Al-Si-Cu high-strength die-casting alloys suitable for castings with thin walls and large areas. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of these 3xxx series alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

383.0, 384.0, and A384.0: Al-Si-Cu High-Strength Die-Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 567–568, https://doi.org/10.31399/asm.hb.v02b.a0006576