This datasheet provides information on key alloy metallurgy, mill product specifications, processing effects on physical and mechanical properties, and applications of high-strength aerospace alloys 2024 and Alclad 2024. It contains tables that list values of tensile property limits for 2024 sheet, plate, and round product forms. Figures illustrate the effect of stretching and aging on toughness of the 2024 sheet and the effect of temperature on tensile properties of 1.0 mm thick Alclad 2024-T3 sheet.